Problem with filtering the solution from ore

Gold Refining Forum

Help Support Gold Refining Forum:

This site may earn a commission from merchant affiliate links, including eBay, Amazon, and others.

mohamedmsud

Member
Joined
Nov 9, 2018
Messages
16
Hello my friends
After a great deal of trouble, I was able to use Aqua Riga on soil . This was done very successfully. The results were impressive. The samples were from 1 kg to 5 kg. The problem that is now facing me is in the filtration. I used to extract the solution using filter paper and cotton.


Now I have decided to work in large quantities to expand the project, any suggestions for filtering, with larger quantities.
thank alot
 
mohamedmsud said:
i did bro ... but it takes long time

Filtering is usually the longest part of the job. Large buchner funnels with a regulated vacuum would help.
 
Thank you all .. I have created one of the methods using ordinary materials such as plastic, sand and shale, to get a pure solution of large quantities of ore .
 
Hi , you must have a press filtre or an a smiless idea call rotary filter , when you get the principal how it work you will made it
 

Attachments

  • How-to-install-a-concentrate-filtering-system-near-thickener.png
    How-to-install-a-concentrate-filtering-system-near-thickener.png
    38.9 KB · Views: 148
Back
Top