Hello,
I've been processing ceramic CPUs for about a year now and have previously have not refined the Silver Chloride once the solution has been cooled on ice, in February I'll be running 10-15KG of ceramics and would like to try reclaiming the silver as well.
I've read that the Silver Chloride is meant to be dissolved with Nitric acid, turn into a clear blue, then cemented out with copper. Each time I addded to Nitric acid to my Silver Chloride, it would go a murky green and not dissolve. I've also read that I could bathe the CPUs in ntiric acid before putting them in AR to get the silver out then cementing it. What method have you found bed for claiming the silver from ceramic CPUs?
Thank you for your help in advance.
I've been processing ceramic CPUs for about a year now and have previously have not refined the Silver Chloride once the solution has been cooled on ice, in February I'll be running 10-15KG of ceramics and would like to try reclaiming the silver as well.
I've read that the Silver Chloride is meant to be dissolved with Nitric acid, turn into a clear blue, then cemented out with copper. Each time I addded to Nitric acid to my Silver Chloride, it would go a murky green and not dissolve. I've also read that I could bathe the CPUs in ntiric acid before putting them in AR to get the silver out then cementing it. What method have you found bed for claiming the silver from ceramic CPUs?
Thank you for your help in advance.