Hi to all,
Currently we have taken a project on removing impurities by oxygen blowing and oxidizing flux addition to oxidize the base metals.
Need suggestions and clarification about this process like
1. Flux need to use
2. Flux ratios and flux calculation
3. Any other things needed to achieve better results in this trial.
Currently we have taken a project on removing impurities by oxygen blowing and oxidizing flux addition to oxidize the base metals.
Need suggestions and clarification about this process like
1. Flux need to use
2. Flux ratios and flux calculation
3. Any other things needed to achieve better results in this trial.