grainsofgold said:Keep the torch on the top of the bar during and after your pour - you do not want the flame to be on the blue side more yellow- after the bar solidifies take the torch off and then you might want to pickle the bar in a heated pickle solution which will get the crud off-
grainsofgold said:I use a propane and O2 torch - never had an issue=
But always looking to learn more-
In melting silver I know that added o2 is not a great thing-