taborc Active member Joined Mar 28, 2007 Messages 40 Location Lawton O.K. Apr 28, 2007 #1 I got a lot of white stuff in the bottom of my cell what is it? All I put in it was gold plated stuff
I got a lot of white stuff in the bottom of my cell what is it? All I put in it was gold plated stuff
D darkelf2x1 Well-known member Joined Apr 7, 2007 Messages 48 Apr 29, 2007 #2 i think its silver chloride, is it crystalline?
taborc Active member Joined Mar 28, 2007 Messages 40 Location Lawton O.K. Apr 29, 2007 #3 no it looks like little white specks
taborc Active member Joined Mar 28, 2007 Messages 40 Location Lawton O.K. Apr 29, 2007 #4 o yea + the black the gold LOL!!