These prices are based on cashforscrapcomputers.com prices.
This a very basic breakdown of this unit. No trimming, cutting or sorting.
Poweredge 2650
3 HDD= 5.35lb/ $3.74
3 gold ram= 2.25oz/ $1.87
Small duel socket MB= 3lb/ $7.65
Peripheral grade boards= 1lb 5.75oz/ $1.75
Green fiber with heatsinks= 1.5oz/ $1.35
Fingered cards= 2.5oz/ $.58
Cd drive= 11.85oz/ $.11
Fans which i get motor price for= 1lb 6.7oz/ $.50
Clean AL heatsinks= 2lb 7.4oz/ $.98
FE steel= 24.2/ $1.45
Total profit of ($19.98) thats i you got it for free. Took roughly 10 minutes
There was room for 2 long skinny PSUs but they were not present so weight and scrap price calculation is not present. But at .27 per/lb i do know they weigh over a pound a piece.
This a very basic breakdown of this unit. No trimming, cutting or sorting.
Poweredge 2650
3 HDD= 5.35lb/ $3.74
3 gold ram= 2.25oz/ $1.87
Small duel socket MB= 3lb/ $7.65
Peripheral grade boards= 1lb 5.75oz/ $1.75
Green fiber with heatsinks= 1.5oz/ $1.35
Fingered cards= 2.5oz/ $.58
Cd drive= 11.85oz/ $.11
Fans which i get motor price for= 1lb 6.7oz/ $.50
Clean AL heatsinks= 2lb 7.4oz/ $.98
FE steel= 24.2/ $1.45
Total profit of ($19.98) thats i you got it for free. Took roughly 10 minutes
There was room for 2 long skinny PSUs but they were not present so weight and scrap price calculation is not present. But at .27 per/lb i do know they weigh over a pound a piece.