gold plating

Gold Refining Forum

Help Support Gold Refining Forum:

This site may earn a commission from merchant affiliate links, including eBay, Amazon, and others.
Download Hoke and read it.
Read safety section and guided tour on this forum.
Search for AP or sulfuric cell (depending on what kind of gold plated scrap you have).

Many succesful beginners start with AP. Sulfuric cell is much more dangerous.
 
i read all cm hokes after 2 weeks but i didn't fount anything about plating gold and he contain 24-k gold and the plating water contain cyanour, nitric, and b sulfate how can i get my gold back
 
Depends on the nature of the plating solution. Some can be difficult, if not impossible, to extract. However, in most cases, powdered zinc should make a full recovery. You may also achieve your goal by simply plating all of the values from the solution, using an inert anode.

Harold
 
NobleMetalWorks said:
Are you trying to get gold out of a gold plating solution? Or gold plated items?

If it is a gold plating solution, can you give the composition?

Scott

it is a gold plating solution that contains cyanour, nitric acid and bisulphate and 24 kt gold. how can i get the gold out?
 