How well would this work on large gold plated aluminum housings (nickle underplate)
http://www.technaflora.com/indexProduct.php?ID=114
Claims to be 5-10% nitric. Looking for a way to remove the plating from these http://goldrefiningforum.com/phpBB3/viewtopic.php?t=20355
I haven't had time or the place to setup a cell, yet.
If I just sit the housing in this pH down would it attack the aluminum enough to get the gold off or do I need to concentrate it down?
Thanks
http://www.technaflora.com/indexProduct.php?ID=114
Claims to be 5-10% nitric. Looking for a way to remove the plating from these http://goldrefiningforum.com/phpBB3/viewtopic.php?t=20355
I haven't had time or the place to setup a cell, yet.
If I just sit the housing in this pH down would it attack the aluminum enough to get the gold off or do I need to concentrate it down?
Thanks