hi all im doing my first batch of gold fingers i was wondering if it was ok to use 36% hydrochloric acid instead of 32%
 
ok ive made up my solution of hydro acid 36% and copper II chloride to strip the gold foils of the fingers.. it seems to be working
i also have a heap of gold pins.. i have read alot of stuff about it but there is so many ways to do this...
im going to do AR with 36% hydro acid 1:1 mix with water and nitric acid probably only 3 or so mills and make it about 60-80'C... dose this look like im on the right track theres so much to read and it gets a little confusing... :)
 
Don't dissolve gold plated pins in AR, unless you mean kovar pins that are attached to ceramics. Remove the base metals first by CuCl2 or remove the gold selectively by a sulfuric cell.

Regarding the HCl 36%, I don't like it because of the nasty fumes. I would always dilute it to under 25-30%, if possible.
 