jamiebridges7
Member
- Joined
- Aug 13, 2018
- Messages
- 7
so i have a larger batch of mixed plated pins i put into my 5l beaker maybe about 2000 grams or so give or take that i covered with distilled water and added maybe 500ml of nitric acid and let the reaction run threw. everything was fine and went per usual until i added more nitric about another 500ml. the solution originally was a nice blue. i went and got some food and when i came back it was brown.