I did my first cook and pour. Some online videos and this forum nspired me to go for it. My bar weighs 8.115 toz, I was wondering if you have come across a reddish brown tint with goldi swirled around your bar, and the top is always dark and has black spots when I torch it.I dont think I am pouring correctly or using the correct torch. I am going to try selling to a wholesaler, so I was trying not to AG the gold. I tried to honeycomb it to rid all base metals to try and make it about 99%. I have a nice electric furnace that goes up to 2500F, but the bars look 2 toned...I did a scratch test and it came back above 22k....Any suggestions?
Could I remelt it and cornflake it in water then AG it? Thanks
Is my pour just bad? I use the yellow tank mag/pro
Could I remelt it and cornflake it in water then AG it? Thanks
Is my pour just bad? I use the yellow tank mag/pro