I'm looking for advice on the separation of gold precipitate from a yellow precipitate that is possibly NaPd(SO3)*2H2O
The mixed precipitate was from acid/ bleach chlorination on an ore that contained some nitrates when I was first learning to process it. The precipitates were dropped with SMB.
Any help would be appreciated, I have around 150g of the mix that I would like to salvage at some stage and I've been reading this forum till my head hurts :lol:
The mixed precipitate was from acid/ bleach chlorination on an ore that contained some nitrates when I was first learning to process it. The precipitates were dropped with SMB.
Any help would be appreciated, I have around 150g of the mix that I would like to salvage at some stage and I've been reading this forum till my head hurts :lol: