Hi all, not sure where to put this as I found no direct references to plated SS. If this thread is not useful, please delete.
I have 3-1/2 lbs of gold plated stainless steel coax connectors.
It has 50u" plating over 303 steel.
What is the best way to lift off the gold.
Tried melting first - ss kinda not cooperative.
Nitric no real help either.
How about lifting in Acid Peroxide?
I have 3-1/2 lbs of gold plated stainless steel coax connectors.
It has 50u" plating over 303 steel.
What is the best way to lift off the gold.
Tried melting first - ss kinda not cooperative.
Nitric no real help either.
How about lifting in Acid Peroxide?