so i have lots of plastic chips and circut boards with gold, but i do not know how to get the foils out...
Very good advice,but I would highly suggest you well what you have.Plastic chips contain very little,to no,precious metals,and the boards will cost you more to process them,than you will recover in metals.Sell.jrmycooke said:Trust me, anyone here can tell you how to do it, but you need to know why the reactions and exchanges are happening to fully understand it and be safe at the same time.
ok so if i dont get the gold out of the chips i still have a lot of the green circut boards and little plastic pieces with gold in them go how i get the foils off?mic said:Very good advice,but I would highly suggest you well what you have.Plastic chips contain very little,to no,precious metals,and the boards will cost you more to process them,than you will recover in metals.Sell.jrmycooke said:Trust me, anyone here can tell you how to do it, but you need to know why the reactions and exchanges are happening to fully understand it and be safe at the same time.
Enter your email address to join: