N NH4+ New member Joined May 26, 2012 Messages 3 Location Ontaio May 26, 2012 #1 Hello, I've looked but cant find the answer using search. Can I use Sodium Sulphite instead of SMB for precipitation of gold? I have some already but no SMB. If the answer is yes, will the procedure change? Please /Thanks..........
Hello, I've looked but cant find the answer using search. Can I use Sodium Sulphite instead of SMB for precipitation of gold? I have some already but no SMB. If the answer is yes, will the procedure change? Please /Thanks..........
goldsilverpro In Remembrance Moderator Emeritus Joined Mar 30, 2007 Messages 7,961 Location Benton, Arkansas May 26, 2012 #2 I have always used sodium sulfite to precipitate the gold. Works great.
N NH4+ New member Joined May 26, 2012 Messages 3 Location Ontaio May 26, 2012 #3 Awesome! Thanks for the reply.