There is no gold dissolved in the sulfuric acid. None. All the gold has already been dropped, automatically, during the stripping.Metaphore said:Could someone point me to a tutorial on dropping gold out of sulfuric acid electrolyte after reverse electroplating?
jeneje said:If you do a search for "sulfuric cells" it will give some post to read. Another option is to search Laxersteve's posts he has done a lot of posts on sulfuric cells.
Hope this helps.
Ken
goldsilverpro said:There is no gold dissolved in the sulfuric acid. None. All the gold has already been dropped, automatically, during the stripping.
FrugalRefiner said:Try a search for the words black powder, with author lazersteve.
Searching becomes much easier the more you read the forum. You may not remember where every post is, but you tend to remember some of the terms used and which authors posted them.
Dave