Nice article, they really go into details for the processes. I even saw the word "tenor" used for silver content in the electrolyte in a silver cell. It's not only Dean that is using it. :)

Göran
 
Jordan1 said:
Great read GSP,

What book is that out of?
I have no idea. The link just gave that one chapter, as you see it.

Here's where I got it. Seems like it was a conference publication, put out by Saimm.

http://www.saimm.co.za/Conferences/ExtractiveMetallurgyOfGold/0615-Chapter10.pdf
 
4Metals posted this:

"The Extractive Metallurgy of Gold in south Africa by Stanley details specifics to the process used at the Rand refinery."


http://goldrefiningforum.com/phpBB3/viewtopic.php?f=60&t=5842&p=50495&hilit=THE+EXTRACTIVE+METALLURGY+OF+GOLD#p50495



https://books.google.com/books/about/The_Extractive_Metallurgy_of_Gold_in_Sou.html?id=elvsAAAAMAAJ
 