snoman701 said:
Topher_osAUrus said:
Additionally, waste treatment is significantly less with CN.
Win win win
I don't believe that to be the case once you operate as a business, as it's a listed waste.
That wasnt the point, I wasn't saying "oh just dump it, its in nuts and bugs, a la natural, she'll be alright" -oh no, not in the least.
I meant that for running 30 lbs of pins, its much cheaper to treat the waste for CN than nitric leaching.
Its >5gal vs 60+ gal
A few gal of bleach, vs many kilos of lye or lime
And.. A 5 gallon bucket vs a 55gal drum just sounds so much more appealing as far as a work task of waste treatment.
Really, the acid would probably be more than that, since 1 gal dissolves 2lbs ish, plus the 50-50 dilution, rinses, etc.. Its probably closer to 75.