A
Anonymous
Guest
I am very happy to see that someone has taken the initiative to get a gold refining forum up and going congrats. I personally have been refining close to 2 years now and very much enjoy this as a hobby. I have had some success as well as some disappointments. I have found that refining is a never ending learning process which for me makes it all the more interesting. I primarily use the Ammen books for reference but I would like to get my hands on the Hokes refining book. As far as refining I use AR methoud but would like to start expermenting with a reverse plating cell. Anyway hello all and I look forward to sharing ideas with you all.