This is an iron/gold/? specimen from a mine in Guanajuato, Mexico. Streak is yellow and black; hardness about 3, weight, 37.7 grams. Attempted to clean it with hcl, but the longer it sits afterward, the more it rusts. Also it had a bad sulfur smell, so I roasted it. The surface is rough. My question is how to improve the look, reduce the rusting, and keep it from falling apart as the gold appears to be tiny specks held together by....? Or, am I way off the mark??gold specimen 7-7 3 001.JPGgold specimen 7-7 3 002.JPGgold specimen 7-7 3 003.JPG
 
Take a small sample, a gram will do, crush, roast and dissolve with AR. Test with stannous and see if it really has some gold in it.

A sticky at the top of the prospecting section has lots of easy field tests like that.
 
Hi my name Yvonne would like a little help with these rocks I got would like some feedback on what they might be
 

Attachments

  • IMG_0793.JPG
    IMG_0793.JPG
    2.7 MB · Views: 49
  • IMG_0791.JPG
    IMG_0791.JPG
    2.6 MB · Views: 49
  • IMG_0792.JPG
    IMG_0792.JPG
    2.4 MB · Views: 49
  • IMG_0790.JPG
    IMG_0790.JPG
    2.7 MB · Views: 49
  • IMG_0789.JPG
    IMG_0789.JPG
    2.5 MB · Views: 49

Latest posts

Back
Top