I’ve said it previously but the physiology of chemistry and refining is something I think all newcomers should ponder.
Having had a fairly successful monetary run with my batches... I was stung this week quite hard.
I purchased 50 grams of “9ct” hallmarked items. The reality was they were 1/5 at the very best. I believe some less.
I have just about broke even, probably lost 50£ or so when you factor in time.
It’s not a nice feeling when you get to the end and you are 3 times under your anticipated weight. I believe experiences like this can make people never try again.
I tend to shout when I have a win so I thought I’d share my recent loss.
Having had a fairly successful monetary run with my batches... I was stung this week quite hard.
I purchased 50 grams of “9ct” hallmarked items. The reality was they were 1/5 at the very best. I believe some less.
I have just about broke even, probably lost 50£ or so when you factor in time.
It’s not a nice feeling when you get to the end and you are 3 times under your anticipated weight. I believe experiences like this can make people never try again.
I tend to shout when I have a win so I thought I’d share my recent loss.