No not a Walter White special.
But the way one should reflux certain robust elements in a controlled manner.
In a way that lets you mitigate the spread of any harmful contaminates.
Quite a basic system, a beaker with a watch glass is not nearly adequate to the task in most circumstance.
But what have I finally gotten around to processing?
No, I burnt anything relating to the Pain by name and Payne by nature and had the ashes then blessed by priests.
An interesting study of Narcissistic personality disorder, but that was about it.
But possibly the correct element, but from our trade sources not specialist superalloy.
This is why I enjoy making a living like this.
I was expecting Pt as I was processing my silver cell slime.
I have already harvested quite a bit of Pd from my cell electrolyte using DMG.
So was expecting to have had a good split in the cell.
But no!
I have found absolutely no Pt and yet more Pd.
Evidently most of the rings and dental alloy I have run did not have any platinum at all.
Next to drop.