Studio721
Member
- Joined
- Feb 5, 2021
- Messages
- 6
Hey guys! Not sure if you are familiar with Juul pods, it’s a pod that goes on top of a disposable cigarette. These pods have trace amounts of gold on the bottom connection side. I run my chemical wash the same way I would any other material I’m extracting that day. For some reason the solution I always use, is having a tough time with these pods, while it is working...I’m noticing after 48 hours hardly any significant impact is being made. With this same solution come the 48 mark my materials are pretty much always ready for extracting. Any ideas on why this particular material is resisting the acid wash?
Sent from my iPhone using Tapatalk
Sent from my iPhone using Tapatalk