M Marvinm4u Member Joined Oct 10, 2020 Messages 13 Mar 10, 2021 #1 I've started processing RAM and end up with a BUNCH of tiny MLCCs, although very little by weight. As a general rule, how much should I save up before bothering to process? (Ignoring whether they are magnetic or not). Thanks, MarvinM
I've started processing RAM and end up with a BUNCH of tiny MLCCs, although very little by weight. As a general rule, how much should I save up before bothering to process? (Ignoring whether they are magnetic or not). Thanks, MarvinM
kjavanb123 Well-known member Joined Apr 1, 2009 Messages 1,743 Location USA Mar 11, 2021 #2 Hi Last time I ran a test on Rams mlccs, I got 1g silver and 0.03g of Pd per kg of those. Hope that helps.
Hi Last time I ran a test on Rams mlccs, I got 1g silver and 0.03g of Pd per kg of those. Hope that helps.