The ore come from a mine in southern Nevada . Have had four asst done and x-ray the ore is rich.I have ran 74lbdown 100 fine and got 21/2 oz off metal. There is 100 ton on the surface and probably 2to3 times below surfac and there is a green gray material in vines this comprise 40 ton on surfac. Have been have trouble getting some to refiner is sale it. The last three said that they could do it came down to they where scraper didn't know about mine ore so I need help locating some one to process this ore. If you can help email me [email protected]
 