kadriver
Well-known member
Hello:
I am trying to learn how to produce some clean SO2 gas for precipitating pure gold from an aqueous solution of goldIII chloride.
This reaction can also be produced by adding sodium metabisulfite to the goldIII chloride solution.
But it is thought that the clean gas, bubbled through the goldIII chloride produces a cleaner precipitation with less drag-down of other metals (if present in the goldIII chloride solution).
I can get the gas from my gas supplier, but they want a rental fee on the container of $0.50 per day.
I have all the equipment needed to make the gas.
Can I use sodium metabisulfite (Na2S2O5) mixed with hydrochloric acid to make some clean SO2 gas suitable for clean precipitation of gold from a solution of goldIII chloride?
Should sulfuric acid be used instead of hydrochloric acid?
Should the gas be scrubbed or cleaned through a bubbler prior to being used to precipitate the gold?
Any help here would be greatly appreciated
kadriver
I am trying to learn how to produce some clean SO2 gas for precipitating pure gold from an aqueous solution of goldIII chloride.
This reaction can also be produced by adding sodium metabisulfite to the goldIII chloride solution.
But it is thought that the clean gas, bubbled through the goldIII chloride produces a cleaner precipitation with less drag-down of other metals (if present in the goldIII chloride solution).
I can get the gas from my gas supplier, but they want a rental fee on the container of $0.50 per day.
I have all the equipment needed to make the gas.
Can I use sodium metabisulfite (Na2S2O5) mixed with hydrochloric acid to make some clean SO2 gas suitable for clean precipitation of gold from a solution of goldIII chloride?
Should sulfuric acid be used instead of hydrochloric acid?
Should the gas be scrubbed or cleaned through a bubbler prior to being used to precipitate the gold?
Any help here would be greatly appreciated
kadriver