Larger tilting furnace

Gold Refining Forum

Help Support Gold Refining Forum:

This site may earn a commission from merchant affiliate links, including eBay, Amazon, and others.
I noticed the play button for the video is white on a white t shirt. Just tap the center of his shirt and the video will play.

Sent from my LG-H872 using Tapatalk

 
The exhaust hood is up! Now we layout and build a base plate for the furnace to set on.

https://photos.app.goo.gl/geVcT8bmVgcFHrHH9
Sent some steel plate off to be waterer cut for the reinforcement structure.

Also I got some used hydrolic cylinder for the tilt mechanism and to swing the roof off. I sent them in for a rebuild.

As soon as they come back I will post some updates.

Sent from my LG-H872 using Tapatalk
 
Shark said:
Keep posting updates, I find them very interesting.

Ditto . . .

I am really interested in what PM, noble or commodity metal you plan on doing your "tilt and pour" with? That is one heavy-duty "backyard" project if you're a hobbyist.

Please be setting up your operation in an NV local so I don't have to feel so lonely here in Northern CA :cry:

James :D
 
Cosmetal,

I plan to "employ" the furnace recovering silver from slag and processing silver from a smelting operation that uses it as a collector metal. On it's days off I want to process scrap copper from a variety of sources.

Shark,

Thanks. I will keep updating all the way through the first few heats.

My water jet pieces came in so I will have more video soon. In the meantime here is a short clip of the foundation platform installation.

https://photos.app.goo.gl/votyoH8C4bZtm3ea7
Sent from my LG-H872 using Tapatalk
 
Starting to take shape. It has a 1,000,000 BTU burner.

Plates came back from the water jet company. Everything fit!

I am burning the easy profiles with a track torch myself.

Everything but the 4 x 4 x 1/4 wall tube and the plate from the water jet company is scrap.

https://photos.app.goo.gl/gA7Vmxesid5fPsPa9
Time for supper.



Sent from my LG-H872 using Tapatalk
 
"Planning to process any cats?"

Göran

Shhh... I will lose my foreman.

Sent from my LG-H872 using Tapatalk

 
Grind, grind, grind it's back to the grind.

https://photos.app.goo.gl/VevriEujdmvBXTxa7
Grinding the welds doesn't just make it look good. It exposes any deficiency int the welds so they can be rewelded. (Not saying how many I had to rework : )

Should have set in the stands and on the stop post soon.

I found a good deal on ebay for the hydrolic pump, tanks and valves. I will post some pics when I get it in.

Sent from my LG-H872 using Tapatalk
 
Here is a cad file of a mixer dumper to charge the furnace. I found a new old stock Parker hydraulic actuator on ebay that will run off the same hydraulic pump and tank the tilt the furnace and swing the lid.

f083954b83c6fa858d5041417cc59cb2.jpg


Sent from my LG-H872 using Tapatalk

 
This is like watching a reality show... can't wait for the first melt. :D

Göran
 
It will be awhile yet. But I will keep updating as I go. Including the first pour.