I retorted impregnated mercury for the first time,I now have a clump of gold and silver amalgamation.how do I desperate them?
Sheilareid said:I retorted impregnated mercury for the first time,I now have a clump of gold and silver amalgamation.how do I desperate them?
See Attaching Images or Files, Working with Attachments.Sheilareid said:Thank you for the advice.I am new to this site,and haven't figured out posting pictures yet.