By metal weight by far the largest percentage but the variables in your question probably means no meaningful answer can be given, the variables are is the board populated and if so what with and then how densely populated, has all steel and Aluminium been removed.
 
Thanks for your reply. wel, I want to know that, i've 200 kilo mobile pcb board, which was before i recovered gold from this pcb board with A/P process....!
 
Trinity358 said:
Thanks for your reply. wel, I want to know that, i've 200 kilo mobile pcb board, which was before i recovered gold from this pcb board with A/P process....!

Then all the copper would not be left on the boards after A/P.
 
Cu can be recovered with iron from AP process. So at 200 Kg....you will have 15-20 % Cu......that about 40 Kg.
 