Post by Raza shahid » November 10th, 2018, 6:24 pm

Hi friend i need some help of yours to get pdcl2 brown powder or brown salt i have refined pd salt from mlcc and at the end of chlorination process i got some yellow salt may be ammoniumhexachloropalladate, but i need pdcl2 can u please help to achieve this i think calcing process can evolve ammonium chloride to get pure pdcl2. But i may be wrong i need to know the right way, it will be appreciated.

Lino1406
Active Member
Posts: 1374
Joined: November 1st, 2007, 12:56 pm
Country of Origin: Israel
Location: Israel
Contact:

Re: Pdcl2. Brown color anhydrous salt

Post by Lino1406 » November 10th, 2018, 10:58 pm

Ammoniumhexachloropalladate, is red brown. What is the special need for PdCl2 ?

Raza shahid
Member
Posts: 9
Joined: August 15th, 2018, 6:41 pm
Country of Origin: Pakistan

Re: Pdcl2. Brown color anhydrous salt

Post by Raza shahid » November 11th, 2018, 9:03 am

Need pdcl2 to active the abs plastic for electroplating basicly for activator. i have yellow salt palladium followed by gold n scrape. Need help to achieve pdcl2.

User avatar
Palladium
Active Member
Posts: 5316
Joined: January 17th, 2008, 1:54 am
Location: USA

Re: Pdcl2. Brown color anhydrous salt

Post by Palladium » November 11th, 2018, 10:55 am

The difference between stupidity and genius is that genius has its limits. Albert Einstein
1. Refining Precious Metal Wastes C.M. Hoke http://tinyurl.com/mfnyhs
(REV) (Free Download)
2. Get the (FREE) Gold Refining Forum Handbook VOL 1 here >> http://tinyurl.com/nyutnp
3. Get the (FREE) Gold Refining Forum Handbook VOL 2 (Final) here >> http://tinyurl.com/y9w5y73
4. Silver cell setup video here (FREE) >> https://tinyurl.com/jhzadse
ALL FREE-----ALL THE TIME

Lino1406
Active Member
Posts: 1374
Joined: November 1st, 2007, 12:56 pm
Country of Origin: Israel
Location: Israel
Contact:

Re: Pdcl2. Brown color anhydrous salt

Post by Lino1406 » November 11th, 2018, 11:16 am

As far as I know, activation = metallization is done by PdCl2 solution and stannous chloride solution. Therefore I suppose any Pd compound solution will work - of course experimentation and optimization is needed

Raza shahid
Member
Posts: 9
Joined: August 15th, 2018, 6:41 pm
Country of Origin: Pakistan

Re: Pdcl2. Brown color anhydrous salt

Post by Raza shahid » November 11th, 2018, 5:09 pm

In companies pdcl2 is strongly recomended to make solution because of quality, palladium salt of chloride is much better then any other pd salt. For solution.

Lou
Active Member
Posts: 4454
Joined: November 4th, 2007, 5:28 pm
Country of Origin: USA
Location: Rhodia Drive

Re: Pdcl2. Brown color anhydrous salt

Post by Lou » November 12th, 2018, 9:50 am

Please see that thread.
Like chemistry? Try http://sciencemadness.org/talk

All that glitters is not gold. Occasionally it's rhodium :)

ashir
Active Member
Posts: 121
Joined: August 17th, 2018, 1:01 pm
Country of Origin: pakistan

Re: Pdcl2. Brown color anhydrous salt

Post by ashir » January 5th, 2019, 11:29 am

the given link by palladium is best answer of your question, but keep in mind , it will need a high grade proper cham lab with advance equipment and safety,
keep this math always written in front of your wall

Palladium weighs 106.42 grams per mol. Chlorine is 35.453 g/mol. There are twice as many chlorine atoms as there are palladium atoms. So, add them all together as follows: 106.42 g/mol + 2(35.453 g/mol) = 177.34 g/mol for the anhydrous material. Palladium constitutes by mass, 106.42 g/mol Pd / 177.34 g/mol PdCl2 *100 = 60% by mass.