Copper mixed with pgm in solution

Post by Slaughlin79 » November 10th, 2018, 7:24 pm

Is the only way to separate without dropping the copper with platinum besides electrolysis? I poured my ammonium chloride in solution and platinum dropped and I waited for it to settle and when I went back there is a line green precipitate about a half inch thick layered on top of the platinum. I’ve researched trying to find a way but can only find electrolysis.

Slaughlin79
Active Member
Posts: 61
Joined: December 25th, 2017, 11:35 pm
Country of Origin: USA
Location: Southeast,Texas

Re: Copper mixed with pgm in solution

Post by Slaughlin79 » November 10th, 2018, 7:26 pm

I forgot to say it’s from catalytic converters

Lino1406
Active Member
Posts: 1374
Joined: November 1st, 2007, 12:56 pm
Country of Origin: Israel
Location: Israel
Contact:

Re: Copper mixed with pgm in solution

Post by Lino1406 » November 10th, 2018, 10:30 pm

Platinum - do you mean ammonium hexachloroplatinate?