kt I do a lot with vintage and antique jewelry and cannot find a source for the 9kt test acid. The only sources I have found are in the UK and they cannot ship to the US. I am not as sophisticated as many of your users. Wondering if anyone can offer some help?

jimdoc
Active Member
Posts: 4757
Joined: March 12th, 2007, 10:42 pm
Location: Philadelphia

Re: purchasing test acid for 9kt Gold in the US

Post by jimdoc » March 17th, 2019, 11:25 am

You simply use a known 9k sample along side what you are testing on the touchstone with 10k acid, or whatever you have. Here is a good testing guide;