Post by huntersarrow » March 27th, 2020, 1:36 am

So, being in Australia , the hcl i have is the contaminated kind... the kind that turns red with hydrogen peroxide.

Done my reading and found the thread here relating to this and seems will still be OK to use for AP however will it be OK to use for making stannous? It is 28% and bought from Clarke rubber advertised as filtrite pool acid.

Lino1406
Active Member
Posts: 1629
Joined: November 1st, 2007, 12:56 pm
Country of Origin: Israel
Location: Israel
Contact:

Re: stannous question

Post by Lino1406 » March 27th, 2020, 1:44 am

Mix with stannous chloride and see if color is acceptable (minimal discoloration)

User avatar
g_axelsson
Active Member
Posts: 5140
Joined: November 17th, 2007, 8:46 pm
Location: Sweden

Re: stannous question

Post by g_axelsson » March 27th, 2020, 1:49 am

I'm sure it will be fine. toss in some tin and let it dissolve.

Stannous is used to test for precious metals in dirty solutions, a bit of dirt from the tin or HCl shouldn't matter a lot.
Test it on a barren solution as well on solution with gold chloride and you'll learn how it reacts.

Göran
Visit the GoldRefiningWiki, an online refining encyclopedia.
It also contains an online version of the book "Refining Precious Metal Wastes" by Hoke.

huntersarrow
Member
Posts: 7
Joined: February 26th, 2020, 9:52 pm
Country of Origin: Aust

Re: stannous question

Post by huntersarrow » March 27th, 2020, 3:20 am

Thanks... the contamination is from washing minerals so chemical not physical.