If you plan on using nitrates of any kind, you should rethink charcoal. Those are two of the major ingredients for gunpowder.
 
For me it is most practical to catch gasses in a closed system in the next vessel with a matching reagent before letting them pass through the fume hood.

Another important point is, you should always use small increments of hypochlorite at a time when dissolving gold, added with a pipette at the bottom of the solution, so if you do it right, there won't be much chlorine left over, that can escape.
 
The moderators would like to thank all of the members that contributed to the original thread upon which this thread was based, as well as those that asked questions showing what was missing. Because of the extra length and interest in this thread we have created the above consolidated version making for an easier read. We encourage all members to read, comment, and ask questions in the original thread, Acid Peroxide Process Information Thread Q & A's

The Library threads should not be considered to constitute a complete education. Instead, they're more like reading a single book on the subject of recovery and refining. There is so much more information on the forum, and it is impossible to include it all in these condensed threads. Members are strongly encouraged to read the rest of the forum to round out their education.
 