AP solution turns clear when heated

Gold Refining Forum

Help Support Gold Refining Forum:

This site may earn a commission from merchant affiliate links, including eBay, Amazon, and others.

dervishh

Well-known member
Joined
Nov 11, 2022
Messages
52
Location
Mobile Alabama
I started a small batch of BGA chips in AP and started using heat for the first time. I noticed the solution turned crystal clear when the temp got hot the after turning off the heat it went right back to the normal familiar yellow. Anyone know why?
 
I started a small batch of BGA chips in AP and started using heat for the first time. I noticed the solution turned crystal clear when the temp got hot the after turning off the heat it went right back to the normal familiar yellow. Anyone know why?
I'm think it may be more here.
DId you bubble air through it?
 
Back
Top