Ask for platinum recovery from royal water

Gold Refining Forum

Help Support Gold Refining Forum:

This site may earn a commission from merchant affiliate links, including eBay, Amazon, and others.

JonnaGr

New member
Joined
Nov 15, 2021
Messages
3
Location
Durango
D966C75D-91EC-4D69-A3EF-D28CF6A80887.jpegHi! I'm new to this website. I open this topic because I have a mineral with platinum content. And I am looking to recover the values from royal water. I will annex the platinum values it contains. If someone had information on how to make it or if someone is interested in buying the mineral with the current contents. It would be of great help to me. I look forward to a response from some. I will leave my contact in case anyone has more information. Jonathan Gonzalez Reyes #6182214744 [email protected]. Best regards
 
If Lou is on the forum he may well have some advice but generally ore processing is beyond most on here, Deano might also be of help as his speciality is mining recover.
 
Platinum from royal waters, denox by urea or sulphamic acid and cement with Zn. Some prefer precipitation by ammonium chloride followed by melting
 
Back
Top