So the first cell I made was the same design as SREETIPS, my issue was because I was inconsistent with the Power supply, it depleted my electrolyte rather quickly and stopped moving current then the solution turned quite blue.

This time I actually bought a power supply so that I can run it at a set voltage, but my question is what is a good molarity for the electrolyte… I’ve seen anywhere from .5 to over 2.0 M AgNO3. I was going to make the electrolyte from dilute nitric acid and pure silver rounds.
 