Good Afternoon Everyone,

I’m looking at building my first silver cell and was curious, instead of a graphite block or stainless bowl, can brass be used as the cathode? I’ve been trying to do research on the topic but cannot find any information.

Thanks
 
why would you want to do that? you can't afford the $20 ss bowl? zinc (one of the elements of the brass alloy) is HIGHLY REACTIVE on the reactivity series of metals, and will not like being in your electrolyte.
 
Very very bad idea use a piece of stainless steel or graphite or a stainless bowl or you will encounter problems. If you decide to use stainless steel check it’s not magnetic.
 
Good Afternoon Everyone,

I’m looking at building my first silver cell and was curious, instead of a graphite block or stainless bowl, can brass be used as the cathode? I’ve been trying to do research on the topic but cannot find any information.

Thanks
Welcome to us.
I find that your research amount is on the shy side of what is necessary.
The advice you have been given is good.

Here is for your continuing research:

We ask our new members to do 3 things.
1. Read C.M. Hokes book on refining jewelers scrap, it gives an easy introduction to the most important chemistry regarding refining.
It is free here on the forum: https://goldrefiningforum.com/phpBB3/viewtopic.php?f=54&t=19798
2. Then read the safety section of the forum: https://goldrefiningforum.com/forums/safety.47/
3. And then read about "Dealing with waste" in the forum: https://goldrefiningforum.com/threads/dealing-with-waste.10539/

Suggested reading:
https://goldrefiningforum.com/forums/the-library.101/
https://goldrefiningforum.com/threads/when-in-doubt-cement-it-out.30236/
https://goldrefiningforum.com/threa...le-read-this-before-you-post-about-ore.33333/


Forum rules is here.
https://goldrefiningforum.com/threads/gold-refining-forum-rules.31182/
 
why would you want to do that? you can't afford the $20 ss bowl? zinc (one of the elements of the brass alloy) is HIGHLY REACTIVE on the reactivity series of metals, and will not like being in your electrolyte.
I don’t want to do it, and yes I can afford a $20 bowl. Like I stated, was just curious on what can and cannot be used. If you can’t ask questions, what’s the point of a forum? Thanks for the reply though.
 
I don’t want to do it, and yes I can afford a $20 bowl. Like I stated, was just curious on what can and cannot be used. If you can’t ask questions, what’s the point of a forum? Thanks for the reply though.

Many of the members have long experience in recovery and refining so they forget that new members don’t yet fully understand what reacts to what chemicals , it takes time and lots of reading to get to the starter stage in my opinion .
We actually encourage questions as I’m sure you will not be the only one with the same questions and asking is better than making a complete mess that may leave you feeling like giving up.
Many many processes and other topics are fully discussed here on the forum and we encourage new members to do the basics like reading , or will save much time and grief later.
 

Latest posts

Back
Top