goldandsilver123
Well-known member
- Joined
- Aug 11, 2015
- Messages
- 206
I have been requested to analyze catalytic converters PGM's by XRF.
There are standards available?
Can I make my own standards? Perhaps impregnating the ground converter with synthetic PGM solution then drying it?
This is the spectrum I got with LiF 200 crystal from 10º to 100º, you can see the Pd and Rh peaks but without the standards I cannot quantify it.
The Au peaks are spectral impurities from the tube.
The converter was ground to 200 mesh and pressed with wax at 200 kN.
There are standards available?
Can I make my own standards? Perhaps impregnating the ground converter with synthetic PGM solution then drying it?
This is the spectrum I got with LiF 200 crystal from 10º to 100º, you can see the Pd and Rh peaks but without the standards I cannot quantify it.
The Au peaks are spectral impurities from the tube.
The converter was ground to 200 mesh and pressed with wax at 200 kN.