B big red 211 Active member Joined Oct 9, 2009 Messages 25 Feb 2, 2010 #1 I cut apart a couple of converters and they had a lining on the outside that looks like they have flakes of gold in them. Is that stuff gold?
I cut apart a couple of converters and they had a lining on the outside that looks like they have flakes of gold in them. Is that stuff gold?
Q qst42know Well-known member Joined Jul 16, 2008 Messages 2,963 Location Toledo, Ohio, USA Feb 2, 2010 #2 As well as I can tell they are mica (vermiculite) flakes.