I have come across a small amount of ceramic chips with what seems to be visible bond wires.
Some are a little different, but the visible plating and bond wires look the same. So the question is: how best to process? My gut feeling is to break with a hammer and simply put all of it in AR along with my few cermaic DX486 and drop the gold for re-refining later.
Anyone have other approaches to consider? Cyanide is not an option (yet).