silversaddle1
Well-known member
I had posted a photo of these lids in a FB group for discussion about recovery and values. Some of them say they have good plating and they are worth refining, some have said not so much. I was wondering what the page here thinks. This tray has 18 pounds in it, and were all knocked off green fiber CPU's with gold pins. I also did a few of the green fiber pinless ones, seems not all have the plating, and the one's that do don't seem to have the surface area as the pinned ones did. I never even knew there was gold under the lid until I knocked a few of the lids off. I was removing the lids to see how hard it was to do since the fiber cpu will sell for more money without the lid.