I was wondering what the precious metal content if any on these these are mainly from RAM sticks and motherboards and whatnot. Any information or a point in the right direction on a thread that's already addressing this issue would be greatly appreciated thank you.
 

Attachments

  • IMG_20211016_100127250.jpg
    IMG_20211016_100127250.jpg
    1.4 MB · Views: 39
Good morning,
they are Ball Grid Array I.C. chips (middle/high yield content of gold). The RAM IC have gold wires beneath the black epoxy " belt" in between the metallic balls, easy job to do mechanically with an engraver machine if you do not like the pyrolysis/incineration method.
 