Hello,
i am from greece and i have an electrolysis bath which is full of gold but i can't retrieve it. its about 5 gallons solution and according to my dad it should have about 30grams or 1oz of gold disolve in it..
i haven't got lots of knowledge in the matter. i can do electrolysis. can i collect in a plate the gold in the negative plate?and then melt it to get the gold?
or can i add something to the solution tha will gather the gold in the bottom and then drain it and melt it with borax?
Please help me my friends
Thank you very much in advance
i am from greece and i have an electrolysis bath which is full of gold but i can't retrieve it. its about 5 gallons solution and according to my dad it should have about 30grams or 1oz of gold disolve in it..
i haven't got lots of knowledge in the matter. i can do electrolysis. can i collect in a plate the gold in the negative plate?and then melt it to get the gold?
or can i add something to the solution tha will gather the gold in the bottom and then drain it and melt it with borax?
Please help me my friends
Thank you very much in advance