duke1025
Member
- Joined
- Aug 27, 2020
- Messages
- 19
So i am getting ready to do the tests....
Acquaintance Tests:
Test Tube Tests:
1) weight of metal
2) amount of acid ml
3) heat temperature applied
4) reaction - speed of reaction
5) reaction - total time of experiment
6) color during reaction
7) color of fluid completed reaction
Metal + Acid =
------------
1) Copper & acid -
2) Brass & acid -
3) Bronze & acid -
4) Nickel & acid -
5) Zinc & acid -
6) Tin & acid -
7) Lead & acid -
8) Iron & acid -
9) Bismuth & acid -
10) Titanium & acid -
11) Gold & acid -
12) Silver & acid -
and finally in the end, i will make an AR solution and test each metal as well.
platinum group metals, such as rhodium, palladium, ruthenium, osmium, and iridium etc not included in tests, do not have available for testing.
ACIDS to be test against: Hydrochloric, Sulfuric, Nitric, Caustic Soda (Lye), Salt (sodium Chloride)
What would you add to these tests?
Thanks!
Basic setup: immersion heater, test tube holders, 90 deg inverted clamps, 1/4" threaded rod 14" long, AC lamp dimmer to control heater & a test tube.
Acquaintance Tests:
Test Tube Tests:
1) weight of metal
2) amount of acid ml
3) heat temperature applied
4) reaction - speed of reaction
5) reaction - total time of experiment
6) color during reaction
7) color of fluid completed reaction
Metal + Acid =
------------
1) Copper & acid -
2) Brass & acid -
3) Bronze & acid -
4) Nickel & acid -
5) Zinc & acid -
6) Tin & acid -
7) Lead & acid -
8) Iron & acid -
9) Bismuth & acid -
10) Titanium & acid -
11) Gold & acid -
12) Silver & acid -
and finally in the end, i will make an AR solution and test each metal as well.
platinum group metals, such as rhodium, palladium, ruthenium, osmium, and iridium etc not included in tests, do not have available for testing.
ACIDS to be test against: Hydrochloric, Sulfuric, Nitric, Caustic Soda (Lye), Salt (sodium Chloride)
What would you add to these tests?
Thanks!
Basic setup: immersion heater, test tube holders, 90 deg inverted clamps, 1/4" threaded rod 14" long, AC lamp dimmer to control heater & a test tube.