I'd like to get 95% of spot price, which right now is $1,800oz, so that amounts to $3,251 for this 70.3g. If you're willing to pay more, such as 96%, I have no problem with that.
All buttons are pure except for the very smallest one, it's problematic. It weighs .52g, if pure it would probably be .50g. Not sure what I did wrong with this one but I've re-refined buttons such as this in the past and seen that a mere .02g of impurities is all it takes to render them screwed up.
The .52g button was the last one I refined, it was what had settled out in my stockpot from doing all the other buttons. I'm only guessing but I think I simply did that last refining in too much of a hurry, I've had enough of refining for now, time to put away the beakers for awhile.
I want to ask your opinion about shipping these buttons, is it the responsibility of the buyer, the seller, or a little of both? If say for example I was to buy something online on ebay, I as the buyer would pay for shipping, this is the way it works, so does this make sense to apply here on the forum also?
The last batch of buttons I shipped via FedEx, though I would much rather ship via USPS Small Flat Rate Box if that works for you.
All buttons are pure except for the very smallest one, it's problematic. It weighs .52g, if pure it would probably be .50g. Not sure what I did wrong with this one but I've re-refined buttons such as this in the past and seen that a mere .02g of impurities is all it takes to render them screwed up.
The .52g button was the last one I refined, it was what had settled out in my stockpot from doing all the other buttons. I'm only guessing but I think I simply did that last refining in too much of a hurry, I've had enough of refining for now, time to put away the beakers for awhile.
I want to ask your opinion about shipping these buttons, is it the responsibility of the buyer, the seller, or a little of both? If say for example I was to buy something online on ebay, I as the buyer would pay for shipping, this is the way it works, so does this make sense to apply here on the forum also?
The last batch of buttons I shipped via FedEx, though I would much rather ship via USPS Small Flat Rate Box if that works for you.