Paige
Well-known member
I followed the advise in the previous listing about HCL & H2O2. In that it was mentioned that it was possible for the fingers to dissolve into the solution if you added more H2O2. My fingers have been in solution for about 3 or 4 days and are not completely "done". Some gold still remains. I have added nothing since the first concoction. Am I running the risk of some of the gold going into solution cuz it's been in there so long? If so, can it be precipitated out? Should I put on my rubber gloves and remove the fingers where the gold is completely gone to give the solution less surface to work on?
Thank you for your help.
Paige
Thank you for your help.
Paige