Gold Pin Refining - Solid Gold? Unexpexted Results. Help?

Gold Refining Forum

Help Support Gold Refining Forum:

This site may earn a commission from merchant affiliate links, including eBay, Amazon, and others.
Ok.
On this kind of beads that can be quite misleading.
If you hit a high Gold spot it will skew the result.

How much pins and what kind was smelted?
Only a few, enough to make a half gram bead. Out of curiosity I looked at it through my 1000x loupe and you can clearly see gold and copper (guessing I didn't melt enough to fully blend?)
 

Attachments

  • 2022-12-03_17-15-15-13.jpg
    2022-12-03_17-15-15-13.jpg
    330.8 KB · Views: 0
Back