One connector dismantled. Three parts gold plated. one part tin or silver plated copper. White part nylon.

P1030120.JPGP1030126.JPGP1030128.JPG
 
If using sulfuric cell,you must break the outer tube. Otherways you dont get the gold from inside.
Inner part is hard bronse alloy. It breaks easily with a light hit. Outer tube is softer. it will be flattened if you hit it. I will make test bath when i got some free time. I`ll let you know.
 