So I'm an amateur at this. I've been reading and watching videos and here is what I've got.
Collected 10 pounds of gold fingers. NOT RAM modules, the fingers from them. Soaked in HCL and peroxide to remove the foils. Collected the foils in a container marked with ounces, the foils almost reached to the 3 ounce mark. I know, it's liquid ounces on the container I'm just giving a visual. Further processed the foils in HCL and bleach in a large plastic container, the foils dissolved. Added sodium metabisulfite dissolved in water, about 400 grams in 2 gallons of water. Got the muddy water reaction. It's now been several days and the gold is not dropping, nothing is there. The solution is now dark but translucent sort of like tea. What am I doing wrong? What could I do next? Also, the solution is still producing strong chloride odors. There's a lot of gold in there and I'm getting worried.
Thanks for any help from the experts.
Collected 10 pounds of gold fingers. NOT RAM modules, the fingers from them. Soaked in HCL and peroxide to remove the foils. Collected the foils in a container marked with ounces, the foils almost reached to the 3 ounce mark. I know, it's liquid ounces on the container I'm just giving a visual. Further processed the foils in HCL and bleach in a large plastic container, the foils dissolved. Added sodium metabisulfite dissolved in water, about 400 grams in 2 gallons of water. Got the muddy water reaction. It's now been several days and the gold is not dropping, nothing is there. The solution is now dark but translucent sort of like tea. What am I doing wrong? What could I do next? Also, the solution is still producing strong chloride odors. There's a lot of gold in there and I'm getting worried.
Thanks for any help from the experts.